IMG_8194 (4).jpgIMG_8198.jpg
Guys I'm desperate here.
1)I sanded my table top back down with 80 Grit. Worked up to 180.
2)Applied a single application of gel stain. Wiped off all excess vigorously to avoid any drying problems. Waited 72 hours before proceeding.
3)After 72 hours, I Applied first coat of Semi Gloss ARM R Seal W/ foam brusg thinned 25%. Most soaked in
4)Applied Second coat of SG ARM R Seal W/ foam brush, thinned 15%. Looked pretty good. Way too shiny though, and some dull areas.
5)I figured the third coat would be my last coat. This was the underside of the table, and I wanted to get it done quickly so I applied a full strength coat of satin, with a foam brush, without thinning. I wake up this morning to find this disaster.
In the photo, you can see where I wiped on a small amount of mineral spirits. It looks perfect where I wipe the MS. But as the MS evaporates, it goes cloudy again.
Why did it go so wrong with this last coat? The ONLY thing I can think, is I had a small propane heater running for a while before I shut it off. I wanted to get the garage warmer, since it was 65 degrees yesterday. Can the propane fuel burning in the air be the cause of all this misery?