About log sealer, no retailer in my area has any for sale, and looking at it online is expensive. Ran across a formula once for a wood preservative, had you take a quart of linseed oil, a piece of parafin wax melted, think it was a cup full, and remainder paint thinner, mixed up to make a gallon. Found if you just melted the parafin, and poured it into the thinner, it stayed liquid. So, does anyone make their own log end sealer this way?