View Full Version : Buffing out EM8000 with a Rotex.
Russ Massery
10-21-2006, 4:53 PM
I just finished buffing out a new kitchen table I made. I use Traget coatings Em8000. Which is a waterborne Conversion Varnish. Step1 (first pic) sanding out with 400 grit paper. Step 2 first buffing with Menzerna's DD3 course compound. Step 3 buffing with P16 Prepolishing paste. (no pic can't really tell the differents) Step 3 2L polishing paste. (last pic). I'm very happy with the results. So I stopped there. There is another polishing compound in there line. But I chose to stop there because it was the shine I was going for. Not too glossy. Thanks for looking.......
Ted Calver
10-21-2006, 5:03 PM
Russ,
It looks like you nailed it! This is a project you can be rightfully proud of.
Jim Becker
10-21-2006, 5:51 PM
Nice job, Russ!!
Mark Singer
10-21-2006, 6:15 PM
Nice job....I have used it with paste wax ...first applying it and then buffing out.. works real nice
Jason Roehl
10-21-2006, 8:12 PM
I think you have more polishing to do. I can't count the slats on the venetian blinds in the reflection. :D
Seriously, looks good!
Bob Childress
10-22-2006, 8:58 AM
Good show Russ. That's a nice looking finish!!:)
jeremy levine
10-23-2006, 10:14 AM
Thanks for showing the steps , very nice