Nissim Avrahami
08-20-2006, 4:29 PM
Good day
I made some 36” long panel gluing and a few boards had some cupping.
In the past, I was just banging down the cupping with hammer but I noticed that it leaves some marks from the clamp under the panel (and also hit my finger).
I would like to share with you more gentle idea.
Regards
niki
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG1.jpg
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG2.jpg
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG3.jpg
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG4.jpg
I made some 36” long panel gluing and a few boards had some cupping.
In the past, I was just banging down the cupping with hammer but I noticed that it leaves some marks from the clamp under the panel (and also hit my finger).
I would like to share with you more gentle idea.
Regards
niki
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG1.jpg
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG2.jpg
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG3.jpg
http://i50.photobucket.com/albums/f321/avrahami/panel%20gluing/PG4.jpg