Mark Ross
09-22-2015, 7:33 PM
hackadaydotcom/2015/09/22/drawbacks-of-lased-delrin-and-how-to-slip-around-them/#more-167424
Steve Clarkson
09-23-2015, 7:27 AM
And don't forget that the off gas of delrin is formaldehyde.
Julian Ashcroft
09-23-2015, 1:24 PM
On the same site there's an interesting article about marking stainless steel with a laser after coating the steel with a mixture of plaster and isopropyl.